Table 2 Qualitative analysis of surfaces after electrolysis under different conditions. Three examiners independently scored each surface based on 4 SEM images mean ± SD
Table 2 Qualitative analysis of surfaces after electrolysis
author: Thiha Tin Kyaw,Takao Hanawa, Shohei Kasugai | publisher: drg. Andreas Tjandra, Sp. Perio, FISID
Mean roughness score of 4 SEM images per electrolysis of different charges and currents
Mean all examiners
P value compared to Control
Ex 1
Ex 2
Ex 3
Control
2.00 ± 0.00
2.00 ± 0.00
2.00 ± 0.00
2.00 ± 0.00
-
− 1 A, group I
4.00 ± 0.00
3.00 ± 0.00
3.25 ± 0.50
3.42 ± 0.17
*
− 1.5 A, group I
4.00 ± 0.00
3.75 ± 0.50
4.00 ± 0.00
3.92 ± 0.17
*
+ 1 A, group I
3.25 ± 0.50
3.33 ± 0.58
3.75 ± 0.50
3.44 ± 0.53
*
+ 1.5 A, group I
3.25 ± 0.50
4.00 ± 0.00
3.75 ± 0.50
3.67 ± 0.33
*
− 1 A, group III
2.00 ± 0.50
2.00 ± 0.00
2.00 ± 0.00
2.00 ± 0.17
n.s.
− 1.5 A, group III
4.00 ± 0.00
3.00 ± 0.00
3.00 ± 0.00
3.33 ± 0.00
*
+ 1 A, group III
3.00 ± 0.00
4.00 ± 0.00
3.25 ± 0.50
3.42 ± 0.17
*
+ 1.5 A, group III
3.00 ± 0.00
4.00 ± 0.00
4.00 ± 0.00
3.67 ± 0.00
*
Serial posts:
-
Investigation of different electrochemical cleaning methods on contaminated healing abutments in vitro: an approach for metal surface decontamination
-
Background : cleaning methods on contaminated healing abutments
-
Materials and methods : cleaning methods on contaminated healing abutments
-
Results : cleaning methods on contaminated healing abutments (1)
-
Results : cleaning methods on contaminated healing abutments (2)
-
Discussion : cleaning methods on contaminated healing abutments (1)
-
CLONE-Discussion : cleaning methods on contaminated healing abutments (2)
-
Discussion : cleaning methods on contaminated healing abutments (2)
-
Discussion : cleaning methods on contaminated healing abutments (3)
-
Discussion : cleaning methods on contaminated healing abutments (4)
-
Discussion : cleaning methods on contaminated healing abutments (5)
-
Table 1 pH after electrolysis.
-
Table 2 Qualitative analysis of surfaces after electrolysis
-
Table 3 Composition (%wt) of the surface of the healing abutment
-
Figure 1. The amount of residual contamination
-
Figure 2. Microscopical images of the healing abutments
-
Figure 3. Representative SEM images of healing abutments
| Mean roughness score of 4 SEM images per electrolysis of different charges and currents | Mean all examiners | P value compared to Control | |||
|---|---|---|---|---|---|
| Ex 1 | Ex 2 | Ex 3 | |||
| Control | 2.00 ± 0.00 | 2.00 ± 0.00 | 2.00 ± 0.00 | 2.00 ± 0.00 | - |
| − 1 A, group I | 4.00 ± 0.00 | 3.00 ± 0.00 | 3.25 ± 0.50 | 3.42 ± 0.17 | * |
| − 1.5 A, group I | 4.00 ± 0.00 | 3.75 ± 0.50 | 4.00 ± 0.00 | 3.92 ± 0.17 | * |
| + 1 A, group I | 3.25 ± 0.50 | 3.33 ± 0.58 | 3.75 ± 0.50 | 3.44 ± 0.53 | * |
| + 1.5 A, group I | 3.25 ± 0.50 | 4.00 ± 0.00 | 3.75 ± 0.50 | 3.67 ± 0.33 | * |
| − 1 A, group III | 2.00 ± 0.50 | 2.00 ± 0.00 | 2.00 ± 0.00 | 2.00 ± 0.17 | n.s. |
| − 1.5 A, group III | 4.00 ± 0.00 | 3.00 ± 0.00 | 3.00 ± 0.00 | 3.33 ± 0.00 | * |
| + 1 A, group III | 3.00 ± 0.00 | 4.00 ± 0.00 | 3.25 ± 0.50 | 3.42 ± 0.17 | * |
| + 1.5 A, group III | 3.00 ± 0.00 | 4.00 ± 0.00 | 4.00 ± 0.00 | 3.67 ± 0.00 | * |
- Investigation of different electrochemical cleaning methods on contaminated healing abutments in vitro: an approach for metal surface decontamination
- Background : cleaning methods on contaminated healing abutments
- Materials and methods : cleaning methods on contaminated healing abutments
- Results : cleaning methods on contaminated healing abutments (1)
- Results : cleaning methods on contaminated healing abutments (2)
- Discussion : cleaning methods on contaminated healing abutments (1)
- CLONE-Discussion : cleaning methods on contaminated healing abutments (2)
- Discussion : cleaning methods on contaminated healing abutments (2)
- Discussion : cleaning methods on contaminated healing abutments (3)
- Discussion : cleaning methods on contaminated healing abutments (4)
- Discussion : cleaning methods on contaminated healing abutments (5)
- Table 1 pH after electrolysis.
- Table 2 Qualitative analysis of surfaces after electrolysis
- Table 3 Composition (%wt) of the surface of the healing abutment
- Figure 1. The amount of residual contamination
- Figure 2. Microscopical images of the healing abutments
- Figure 3. Representative SEM images of healing abutments